原料類別 |
烘乾時間
(小時) |
烘乾溫度 (℃) |
料管溫度 (℃) |
|
料管本體溫度 |
PS一般用 |
2 |
75-85 |
190-260 |
180-240 |
HIPS (475) |
1 |
60-70 |
190-260 |
180-240 |
A.B.S |
2-4 |
80-100 |
200-240 |
200-230 |
壓克力一般用 |
2-6 |
80-100 |
200-230 |
180-220 |
P.C |
2-10 |
100-200 |
280-320 |
260-310 |
變性PP即NORYL |
2-4 |
105-120 |
250-300 |
240-280 |
PPO (SE-100) |
2-4 |
85-95 |
250-300 |
240-280 |
硬質PVC |
1 |
60-80 |
175-195 |
165-185 |
SAN即 (AS) |
2-4 |
75-85 |
200-240 |
200-230 |
P.E |
1 |
70-80 |
200-220 |
180-210 |
P.P |
1 |
70-80 |
210-280 |
200-270 |
P.P.S |
4 |
120-140 |
270-290 |
270 |
尼龍6 |
2-10 |
80
|
240-280 |
225-280 |
尼龍6.6 |
2-10 |
80
|
270-310 |
260-280 |
DELRIN (塑鋼) |
2-4 |
80-90 |
190-220 |
180-200 |
鳩拉康 (塑鋼) |
2-4 |
80-90 |
230-280 |
220-270 |
POM (塑膠鋼) |
2-4 |
80-90 |
200-230 |
200-260 |
P.B.T |
4-5 |
130-140 |
210-250 |
210-250 |
R-PET
(PET加纖) |
4-5 |
130-140 |
240-270 |
230-280 |
CA (阿西底) |
2 |
100 |
230 |
200 |
|
|
|